Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2.10 MPa | 305 psi | Parallel to thickness |
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Flexural Strength | 2.10 MPa | 305 psi | @ 15 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SF-200H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 2.10 MPa | 305 psi | @ 15 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SF-200H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 2.10 MPa | 305 psi | Parallel to thickness |
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |