Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 19.0 MPa | 2760 psi | STN EN ISO 178 |
Plastcom PLASTALEN® PQ 82 N 003/1M Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Flexural Strength | 19.0 MPa | 2760 psi | |
Quadrant EPP TIVAR® 1000 ASTL PE-UHMW + specific additives (ISO Data) TIVAR 1000 ASTL, based on a PE-UHMW grade with extremely high molecular weight, has been specifically developed for tough anti-abrasion applications. TIVAR 1000 ASTL shows a higher wear and abrasion.. |
|||
Flexural Strength | >= 19.0 MPa | >= 2760 psi | |
MarkeTech Repton 931 Cordierite Mg-Al-Si Oxide REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Flexural Strength | 19.0 MPa | 2760 psi | |
Kuraray HYBRAR® PP1 Thermoplastic Rubber-Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer LUBRICOMP* YL003C is a compound based on Polyester Elastomer resin containing 15% PTFE. Added features of this grade include: Clean Compound System, Wear Resistant. |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer (Asia Pacific) LUBRICOMP* YL-4030 CCS is a PTFE Lubricated Compound based on Polyester Elastomer resin which has low ionic and low outgassing performance for the Semicon and Internal Hard Disk Drive applications. |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp TH0450D LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific) LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific) LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 2X00858 FP-F (FEP) LNP* THERMOCOMP* 2X00858 is a compound based on FEP resin containing proprietary fillers. |
|||
Flexural Strength | 19.0 MPa | 2760 psi | Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ASTM D790 |
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ASTM D790 |
Lubrizol Estaloc® 59020 Reinforced Thermoplastic Polyurethane Type: Estaloc® 59020 RETPU is a polyester-type reinforced engineered thermoplastic polyurethane (RETPU).Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.. |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ASTM D790 |
Lubrizol ESTALOC® 60155 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol |
|||
Flexural Strength | 19.0 MPa | 2760 psi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 19.0 MPa @Strain 3.50 % |
2760 psi @Strain 3.50 % |
50%RH; ISO 178 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437C30L Calcium Reinforced |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437C40L Calcium Reinforced |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437W10L Wollastonite Reinforced |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437W20L Wollastonite Reinforced |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437W30L Wollastonite Reinforced |
|||
Flexural Strength | 19.0 MPa | 2760 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437W40L Wollastonite Reinforced |