Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 125 MPa | 18200 psi | ASTM D790 |
Polymer Resources PCSF-FR G30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Flexural Strength | 125 MPa | 18200 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF13 IM2 HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Flexural Strength | 125 MPa | 18200 psi | |
Aremco AREMCOLOX™ 502-1800 Machinable Aluminum Nitride Hot-pressed boron nitride – aluminum nitride composite that demonstrates high thermal conductivity, dielectric strength, and abrasion resistance. Readily machined and available in rods from 1/4” t.. |