Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1.19 MPa | 173 psi | ISO 178 |
Multibase TPSiV® 4200-50A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |