Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 110.85 MPa | 16077 psi | ASTM D790 |
E-Polymers SEPAZ® V230B 30% Mineral Filled Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Flexural Strength | 110.85 MPa | 16077 psi | ASTM D790 |
E-Polymers TEKAMID® JN100 PPE+PA66 Filler Reinforced PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |