Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 151.72 MPa | 22005 psi | ASTM D790 |
Lucent Polymers GPC-0202 20 Polycarbonate, Glass Reinforced, Injection Grade Recycled ContentAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 151.72 MPa | 22005 psi | ASTM D790 |
Lucent Polymers GPCB-120 Polycarbonate+PBT, 20% Glass Fiber Reinforced Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 151.72 MPa | 22005 psi | ASTM D790 |
Lucent Polymers L6-140 Nylon 6, 15% Glass Fiber and 25% Mineral Reinforced Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |