Polymer Property : Flexural Strength = 128 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 121 - 128 MPa
17500 - 18500 psi
ASTM D790
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon
Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice..
Flexural Strength 100 - 128 MPa
14500 - 18500 psi
Bulk Molding Compounds BMC T14 General Purpose Molding Compound
BMC T14 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T14 is well suited for injection, transfer or compression molding of intricate parts. Typica..
Flexural Strength 100 - 128 MPa
14500 - 18500 psi
Bulk Molding Compounds BMC A50-MS General Purpose Molding Compound
BMC A50-MS is a medium strength, high appearance, general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A50-MS is well suited for injection, transfer or compres..