Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 127 MPa | 18400 psi | ASTM D790 |
SABIC Innovative Plastics Lexan® LF1520 PC (Asia Pacific) |
|||
Flexural Strength | 127 MPa | 18400 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp DFL329EF PC LNP LUBRICOMP* DFL329EF is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.This data was supplied by .. |
|||
Flexural Strength | 127 MPa @Temperature 150 °C |
18400 psi @Temperature 302 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Flexural Strength | 127 MPa | 18400 psi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (.. |
|||
Flexural Strength | 127 MPa | 18400 psi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK) AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava.. |
|||
Flexural Strength | 127 MPa | 18400 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 5C003 FP-V (PVDF) LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 127 MPa | 18400 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp 9X06477 SPS LNP* Thermocomp* 9X06477 is a compound based on Syndiotactic Polystyrene resin containing Glass Fiber. Characteristics of this grade is Heat Stabilized.This data was supplied by SABIC-IP for the Am.. |
|||
Flexural Strength | 127 MPa | 18400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000 PC (Asia Pacific) |
|||
Flexural Strength | 127 MPa | 18400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® LB-3150GW PC, 15% Glass Filled High Impact High-impact resistant PC/GF that can be used for middle mold frame of LCD TVInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 127 MPa | 18400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-4020 ABS, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 127 MPa | 18400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-4030 ABS, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 127 MPa | 18400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® LB-3150GW PC, 15% Glass Filled High Impact High-impact resistant PC/GF that can be used for middle mold frame of LCD TVInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 127 MPa | 18400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-4020 ABS, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 127 MPa | 18400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-4030 ABS, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 127 MPa | 18400 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp KFI12A Acetal Homopolymer LNP LUBRICOMP* KFI12A is a compound based on Acetal Homopolymer resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABI.. |
|||
Flexural Strength | 127 MPa | 18400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WCP36 PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WCP36 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber, PTFE, Silicone. Added features include; Internally Lubricated, Electrically Conductive. |
|||
Flexural Strength | 127 MPa | 18400 psi | ASTM D790 |
SABIC Innovative Plastics Xenoy® 1760 PBT+PC (Asia Pacific) |
|||
Flexural Strength | 127 MPa | 18400 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp 5C003 LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. Also known as THERMOCOMP* FP-VC.. |
|||
Flexural Strength | 127 MPa | 18400 psi | ASTM D790 |
Plenco 7556 Phenolic, Briquette, Injection Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Flexural Strength | 127 MPa | 18400 psi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Flexural Strength | 127 MPa | 18400 psi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 511 Polycarbonate, Glass Fiber/PTFE, UL Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Strength | 127 MPa | 18400 psi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-0632 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 127 MPa | 18400 psi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (5 mi.. |
|||
Flexural Strength | 127 MPa | 18400 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL329 PC LNP LUBRICOMP* DFL329 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |
|||
Flexural Strength | 127 MPa | 18400 psi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir.. |