Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D-790 |
Plaskolite Optix® CA - 41 FDA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D-790 |
Plaskolite Optix® CA - 41 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 13FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D-790 |
Plaskolite Optix® CP - 41 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D-790 |
Plaskolite West Optix® CA - 41 FDA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
Network Polymers Kepital® F20-52 Description: Natural Acetal Copolymer, Weather Resistance GradeInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 80.9 MPa | 11700 psi | 13 mm/min; ASTM D790 |
PolyOne Edgetek® XT EX3600-0002 UV Black Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
PolyOne Geon™ HTX Ultra LA427Plus Polyvinyl Chloride Alloy (PVC Alloy) Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties based on Geon HTX Ultra LA427Plus Natural 0000Information provided by PolyOne |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
PolyOne Geon™ SF M7100 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP D1000P PC LNP* COLORCOMP* D1000P is an unfilled Polycarbonate. Added feature of this grade is: Exceptional Processing. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D-790 |
Plaskolite West Optix® CA - 41 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX09402 PC LNP* THERMOCOMP* DX09402 is a compound based on Polycarbonate containing Proprietary Filler(s). |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
Styrolution Novodur® HH-112 ABS Novodur HH-112 is a high heat injection molding grade. It provides good heat resistance combined with enhanced stiffness.Information provided by Styrolution |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
Styron Pulse® 2100LG ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP D7002IXH PC LNP* THERMOCOMP* D7002IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces, housings, etc., in healthcare an.. |
|||
Flexural Strength | 80.7 MPa @Thickness 3.20 mm |
11700 psi @Thickness 0.126 in |
Injection Molded; ASTM D790 |
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can .. |
|||
Flexural Strength | 80.4 MPa @Thickness 3.20 mm |
11700 psi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SC 201LV General Purpose Polystyrene CharacteristicsHigh molecular weight grade Good flow properties along with good mechanical strength Easy process ability with good mold release propertiesProcessing Injection moldingApplicationsSuit.. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
Teknor Apex Sinpolene GPP1615/2 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 15% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Flexural Strength | 80.7 MPa @Strain 5.00 % |
11700 psi @Strain 5.00 % |
ASTM D790-10A |
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC) TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products .. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
Westlake Plastics Corzan® II CPVC Sheet Corzan® II CPVC, manufactured from Corzan G2 resin, was developed for use in the construction of wet benches and other cleanroom equipment for the semiconductor industry. It meets Factory Mutual.. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis.. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
Total PSC 536 Polystyrene Polystyrene 536 is a high melt flow; high heat crystal polystyrene. Designed for fast cycle injection molding and for high output, direct injection profile extrusion for foam applications.Informatio.. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 522 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ASTM D790 |
Plaskolite West Optix® CA-41 General Purpose Acrylic Resin Injection Molding Grade Pellets only. Lowest Heat Resistance and maximum flow. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ASTM D790 |
Plenco 2000 Phenolic, Granular, Transfer Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
Polyplastics Duracon® M25-45 Acetal Co-polymer (POM), Weather resistance, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PH0800A PA 6 LNP* THERMOCOMP* PH0800A is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity. |