Mechanical Properties Metric English Comments
Flexural Strength 8.00 MPa
1160 psi
ASTM D790
SABIC MG500026 Linear Low Density Polyethylene for Compounding
Product Description: MG500026 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution primarily suitable for compounding applications. It is in the powder form and h..
Flexural Strength 8.00 MPa
1160 psi
(C 203)
Pyrotek Pyrite B-3 Refractory Board
Pyrotek B-3 is a highly versatile calcium silicate board for use in a variety of machined shapes and general purpose applications. Among its uses, Pyrotek B-3 is established as the industry standar..
Flexural Strength 8.00 MPa
1160 psi
Y-Direction; IPC-TM-650, 2.4.4
Rogers Corporation RO3730 Antenna Grade Laminate
RO3730™ Laminates have the excellent thermo-mechanical properties and electrical characteristics that antenna designers need. The laminates have a dielectric constant of 3.0 and a loss tangent of..
Flexural Strength 8.00 MPa
1160 psi
ASTM D790
SABIC M500026 Linear Low Density Polyethylene for Injection Molding
Product Description: M500026 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to give excell..
Flexural Strength 8.00 MPa

@Temperature 120 °C
1160 psi

@Temperature 248 °F
ASTM D790
BASF Capron® 8224 HSL Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Flexural Strength 8.00 MPa
1160 psi
Olsen; ASTM D747
UBE V210 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
Flexural Strength 8.00 MPa
1160 psi
XD; ASTM D790
DuPont™ Nomex® Type 994, 125 mil Nominal Thickness Rigid Aromatic Nylon Board
Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T..
Flexural Strength 8.00 MPa
1160 psi
XD; ASTM D790
DuPont™ Nomex® Type 994, 250 mil Nominal Thickness Rigid Aromatic Nylon Board
Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T..
Flexural Strength 8.00 MPa

@Temperature 120 °C
1160 psi

@Temperature 248 °F
ASTM Test
BASF Ultramid® 8255 HS PA6 (Dry)
Ultramid 8255 HS is a heat stabilized, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying levels of toughness and fle..
Flexural Strength 8.00 MPa
1160 psi
SAE J949
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 8.00 MPa
1160 psi
ISO 178
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, Conditioned
Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced ..