Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 0.550 MPa | 79.8 psi | 30 g/l |
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionThis is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S332 which will lead the industry in.. |
|||
Flexural Strength | 0.550 MPa | 79.8 psi | Parallel to thickness |
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Flexural Strength | 0.550 MPa | 79.8 psi | Parallel to thickness |
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |