Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 0.330 MPa | 47.9 psi | DIN-EN 12089 |
BASF E-por® 0.025 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |