Polymer Property : Tensile Stress = 9860 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 68.0 MPa

@Strain 10.0 %,
Temperature 0.000 °C
9860 psi

@Strain 10.0 %,
Temperature 32.0 °F
Solvay TECHNYL® A 205F PA66, Conditioned
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Tensile Stress 67.98 MPa

@Strain 0.820 %,
Temperature 0.000 °C
9860 psi

@Strain 0.820 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided ..
Tensile Stress 67.98 MPa

@Strain 0.760 %,
Temperature 40.0 °C
9860 psi

@Strain 0.760 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G30NH BK337 Polyphthalamide (PPA)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It..
Tensile Stress 68.0 MPa

@Strain 11.0 %,
Temperature 23.0 °C
9860 psi

@Strain 11.0 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..
Tensile Stress 68.0 MPa

@Strain 7.00 %,
Temperature 40.0 °C
9860 psi

@Strain 7.00 %,
Temperature 104 °F
ISO 527
BASF Ultradur B 4300 G2 10% Glass Filled PBT
Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Tensile Stress 68.0 MPa

@Strain 4.60 %,
Temperature -20.0 °C
9860 psi

@Strain 4.60 %,
Temperature -4.00 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers