Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 91.4 MPa @Strain 6.00 %, Temperature -40.0 °C |
13300 psi @Strain 6.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring .. |
|||
Tensile Stress | 91.4 MPa @Strain 6.00 %, Temperature -40.0 °C |
13300 psi @Strain 6.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear .. |
|||
Tensile Stress | 91.4 MPa @Strain 1.71 %, Temperature 0.000 °C |
13300 psi @Strain 1.71 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G15HSLR BK031 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR BK031 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |