Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 9.52 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 9.52 MPa

@Strain 102.09 %,
Temperature 100 °C
1380 psi

@Strain 102.09 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.52 MPa

@Strain 40.0 %,
Temperature 80.0 °C
1380 psi

@Strain 40.0 %,
Temperature 176 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 9.52 MPa

@Strain 88.68 %,
Temperature 60.0 °C
1380 psi

@Strain 88.68 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved