Polymer Property : Tensile Stress = 9.20 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 9.20 MPa

@Strain 300 %,
Thickness 2.00 mm
1330 psi

@Strain 300 %,
Thickness 0.0787 in
Type 1, 200 mm/min; Flow; DIN 53504
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE)
OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
Tensile Stress 9.20 MPa

@Strain 47.92 %,
Temperature 100 °C
1330 psi

@Strain 47.92 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.20 MPa

@Strain 45.0 %,
Temperature 80.0 °C
1330 psi

@Strain 45.0 %,
Temperature 176 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.20 MPa

@Strain 195.71 %,
Temperature 120 °C
1330 psi

@Strain 195.71 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 9.20 MPa

@Strain 128.33 %,
Temperature 150 °C
1330 psi

@Strain 128.33 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers