Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 9.03 MPa @Strain 300 % |
1310 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® D6890 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Stress | 9.03 MPa @Strain 300 % |
1310 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® D6785 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Stress | 9.03 MPa @Strain 100 % |
1310 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 4045D Thermoplastic Polyurethane Elastomer Zythane™ 4045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 9.03 MPa @Strain 100 % |
1310 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |