Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 87.17 MPa @Strain 5.71 %, Temperature 150 °C |
12640 psi @Strain 5.71 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 87.17 MPa @Strain 3.31 %, Temperature 150 °C |
12640 psi @Strain 3.31 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |