Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 59.5 MPa @Strain 1.50 %, Temperature 23.0 °C |
8630 psi @Strain 1.50 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 59.5 MPa @Strain 14.0 %, Temperature 40.0 °C |
8630 psi @Strain 14.0 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Tensile Stress | 59.5 MPa @Strain 14.0 %, Temperature 40.0 °C |
8630 psi @Strain 14.0 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Tensile Stress | 59.5 MPa @Strain 9.30 %, Temperature 90.0 °C |
8630 psi @Strain 9.30 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |
|||
Tensile Stress | 59.5 MPa @Strain 0.960 %, Temperature 90.0 °C |
8630 psi @Strain 0.960 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) 43% Glass Reinforced Polyamide 612Zytel 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 59.5 MPa @Strain 2.80 %, Temperature 150 °C |
8630 psi @Strain 2.80 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |