Mechanical Properties Metric English Comments
Tensile Stress 59.0 MPa

@Strain 2.50 %,
Temperature 100 °C
8560 psi

@Strain 2.50 %,
Temperature 212 °F
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY
Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 59.0 MPa

@Strain 2.00 %
8560 psi

@Strain 2.00 %
Solvay TECHNYL® A 217 PA66, DRY
Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim..
Tensile Stress 59.0 MPa

@Strain 3.71 %,
Temperature 120 °C
8560 psi

@Strain 3.71 %,
Temperature 248 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66