Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 85.03 MPa @Strain 2.01 %, Temperature 60.0 °C |
12330 psi @Strain 2.01 %, Temperature 140 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK608 BK509 PBT
(Unverified Data**) Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 85.03 MPa @Strain 8.73 %, Temperature -20.0 °C |
12330 psi @Strain 8.73 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |
|||
Tensile Stress | 85.03 MPa @Strain 2.63 %, Temperature 40.0 °C |
12330 psi @Strain 2.63 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl.. |