Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.70 MPa @Strain 10.0 % |
827 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 5.70 MPa @Strain 17.16 %, Temperature 150 °C |
827 psi @Strain 17.16 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 5.70 MPa @Strain 300 % |
827 psi @Strain 300 % |
ASTM D412 |
ExxonMobil Vistamaxx™ 3980FL Propylene-based Elastomer - High Purity, Low Gel Product Description: Vistamaxx 3980FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us.. |
|||
Tensile Stress | 5.70 MPa @Strain 0.120 %, Temperature 120 °C |
827 psi @Strain 0.120 %, Temperature 248 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |
|||
Tensile Stress | 5.70 MPa @Strain 10.0 %, Temperature 100 °C |
827 psi @Strain 10.0 %, Temperature 212 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |