Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 82.28 MPa @Strain 2.21 %, Temperature 90.0 °C |
11930 psi @Strain 2.21 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po.. |