Polymer Property : Tensile Stress = 81.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 81.0 MPa

@Strain 10.0 %,
Temperature 100 °C
11700 psi

@Strain 10.0 %,
Temperature 212 °F
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY
Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 81.0 MPa

@Strain 4.00 %
11700 psi

@Strain 4.00 %
Solvay TECHNYL® A 217 PA66, DRY
Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim..
Tensile Stress 81.0 MPa

@Strain 19.2 %,
Temperature -40.0 °C
11700 psi

@Strain 19.2 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
Tensile Stress 81.0 MPa

@Strain 0.740 %,
Temperature 0.000 °C
11700 psi

@Strain 0.740 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Tensile Stress 81.0 MPa

@Strain 17.0 %,
Temperature -20.0 °C
11700 psi

@Strain 17.0 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..