Mechanical Properties Metric English Comments
Tensile Stress 79.7 MPa

@Strain 24.0 %,
Temperature 0.000 °C
11600 psi

@Strain 24.0 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..