Polymer Property : Tensile Stress = 7830 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 54.0 MPa

@Strain 3.23 %,
Temperature 23.0 °C
7830 psi

@Strain 3.23 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal..
Tensile Stress 54.0 MPa

@Strain 8.80 %,
Temperature 23.0 °C
7830 psi

@Strain 8.80 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
Tensile Stress 54.0 MPa

@Strain 5.00 %,
Temperature 40.0 °C
7830 psi

@Strain 5.00 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem..
Tensile Stress 54.0 MPa

@Strain 1.10 %,
Temperature 150 °C
7830 psi

@Strain 1.10 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSLR BK420 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin with improved hydrolysis resistance..
Tensile Stress 54.0 MPa

@Strain 1.24 %,
Temperature 23.0 °C
7830 psi

@Strain 1.24 %,
Temperature 73.4 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..