Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 53.92 MPa @Strain 7.92 %, Temperature 0.000 °C |
7820 psi @Strain 7.92 %, Temperature 32.0 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 53.92 MPa @Strain 0.500 %, Temperature -40.0 °C |
7820 psi @Strain 0.500 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 53.9 MPa @Strain 0.280 %, Temperature -40.0 °C |
7820 psi @Strain 0.280 %, Temperature -40.0 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Tensile Stress | 53.9 MPa @Strain 2.40 %, Temperature 0.000 °C |
7820 psi @Strain 2.40 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Stress | 53.9 MPa @Strain 2.08 %, Temperature 90.0 °C |
7820 psi @Strain 2.08 %, Temperature 194 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |