Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 73.54 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 73.54 MPa

@Strain 1.41 %,
Temperature 60.0 °C
10670 psi

@Strain 1.41 %,
Temperature 140 °F
ISO 527
DuPont Performance Polymers Crastin® SK608 BK509 PBT  (Unverified Data**)
Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 73.54 MPa

@Strain 1.41 %,
Temperature 23.0 °C
10670 psi

@Strain 1.41 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G15HSLR BK031 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR BK031 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i..