Polymer Property : Tensile Stress = 7.52 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 7.52 MPa

@Strain 300 %
1090 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-2185 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..
Tensile Stress 7.52 MPa

@Strain 20.0 %,
Temperature 100 °C
1090 psi

@Strain 20.0 %,
Temperature 212 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 7.52 MPa

@Strain 6.47 %,
Temperature 40.0 °C
1090 psi

@Strain 6.47 %,
Temperature 104 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..
Tensile Stress 7.52 MPa

@Strain 6.47 %,
Temperature 40.0 °C
1090 psi

@Strain 6.47 %,
Temperature 104 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers