Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 48.0 MPa @Strain 3.00 %, Temperature 200 °C |
6960 psi @Strain 3.00 %, Temperature 392 °F |
|
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Tensile Stress | 48.0 MPa @Strain 0.500 %, Temperature 0.000 °C |
6960 psi @Strain 0.500 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 48.0 MPa @Strain 50.0 %, Temperature 23.0 °C |
6960 psi @Strain 50.0 %, Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
Tensile Stress | 48.0 MPa @Strain 13.0 %, Temperature 23.0 °C |
6960 psi @Strain 13.0 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | >= 48.0 MPa @Strain 300 % |
>= 6960 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 572D Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |