Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 68.46 MPa @Strain 1.23 %, Temperature 0.000 °C |
9929 psi @Strain 1.23 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G15HSLR BK031 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR BK031 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |
|||
Tensile Stress | 68.46 MPa @Strain 0.600 %, Temperature -40.0 °C |
9929 psi @Strain 0.600 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers |