Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 45.07 MPa @Strain 1.27 %, Temperature 150 °C |
6537 psi @Strain 1.27 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |