Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.48 MPa @Strain 300 % |
650 psi @Strain 300 % |
|
NEU NeuSoft™ 596-50A Medical Ether TPU / SBC blend |
|||
Tensile Stress | 4.48 MPa @Strain 300 % |
650 psi @Strain 300 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9172 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Tensile Stress | 4.48 MPa @Strain 300 % |
650 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TL-90-T3030A-80 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Stress | 4.48 MPa @Strain 300 % |
650 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TL-91-T3056D-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Stress | 4.48 MPa @Strain 0.100 %, Temperature 150 °C |
650 psi @Strain 0.100 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA) Zytel® HTNFR52G20NH BK337 is a 20% glass reinforced, flame retardant, lubricated high performance polyamide resin. It is also a PPA resin and it uses a non-halogenated flame retardant.Information p.. |