Mechanical Properties Metric English Comments
Tensile Stress 4.34 MPa

@Strain 300 %,
Temperature 23.0 °C
629 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ HC MT222 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT222 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT222 has been specially formulated without the use of any plasticize..
Tensile Stress 4.34 MPa

@Strain 300 %,
Temperature 23.0 °C
629 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 6275-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6275-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. New Prod..
Tensile Stress 4.34 MPa

@Strain 100 %,
Temperature 23.0 °C
629 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
Tensile Stress 4.34 MPa

@Strain 0.100 %,
Temperature 150 °C
629 psi

@Strain 0.100 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)  (Unverified Data**)
20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It..