Mechanical Properties Metric English Comments
Tensile Stress 43.0 MPa

@Strain 160 %,
Temperature 23.0 °C
6240 psi

@Strain 160 %,
Temperature 73.4 °F
Solvay TECHNYL® eXten D 437P PA6.10
Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia..
Tensile Stress 43.0 MPa

@Strain 300 %
6240 psi

@Strain 300 %
ASTM D412
Alliance Polymers Zythane™ 6065D Thermoplastic Polyurethane Elastomer
Zythane™ 6065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 43.0 MPa

@Strain 300 %
6240 psi

@Strain 300 %
ASTM D412
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer
Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 43.0 MPa

@# of Cycles 100000 ,
Temperature 180 °C
6240 psi

@# of Cycles 100000 ,
Temperature 356 °F
BASF Ultrason E 2010 G6 30% Glass Filled PES
Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.
Tensile Stress 43.0 MPa

@Strain 50.0 %,
Temperature 23.0 °C
6240 psi

@Strain 50.0 %,
Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66  (Unverified Data**)
Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi..
Tensile Stress 43.0 MPa

@Strain 50.0 %,
Temperature 60.0 °C
6240 psi

@Strain 50.0 %,
Temperature 140 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66  (Unverified Data**)
Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi..
Copyright © lookpolymers.com All Rights Reserved