Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 6.03 MPa @Strain 300 % |
875 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® D6975CT TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Stress | 6.03 MPa @Strain 300 % |
875 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® F7870 TPE, Fire Retardant Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome.. |
|||
Tensile Stress | 6.03 MPa @Strain 300 % |
875 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® D6780 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Stress | 6.03 MPa @Strain 120.12 %, Temperature 150 °C |
875 psi @Strain 120.12 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |