Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 58.0 MPa @Strain 5.00 %, Temperature 0.000 °C |
8410 psi @Strain 5.00 %, Temperature 32.0 °F |
|
Solvay TECHNYL® A 205F PA66, Conditioned Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 58.0 MPa @Strain 4.40 %, Temperature 23.0 °C |
8410 psi @Strain 4.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr.. |
|||
Tensile Stress | 58.0 MPa @Strain 3.38 %, Temperature 23.0 °C |
8410 psi @Strain 3.38 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |
|||
Tensile Stress | 58.0 MPa @Strain 0.800 %, Time 3600 sec |
8410 psi @Strain 0.800 %, Time 1.00 hour |
ISO 899-1 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Tensile Stress | 58.0 MPa @Strain 2.00 % |
8410 psi @Strain 2.00 % |
|
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |