Polymer Property : Tensile Stress = 5414 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 37.33 MPa

@Strain 1.98 %,
Temperature 150 °C
5414 psi

@Strain 1.98 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject..
Tensile Stress 37.33 MPa

@Strain 1.98 %,
Temperature 150 °C
5414 psi

@Strain 1.98 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in..
Tensile Stress 37.33 MPa

@Strain 4.84 %,
Temperature 23.0 °C
5414 psi

@Strain 4.84 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. ..