Polymer Property : Tensile Stress = 5313 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 36.63 MPa

@Strain 0.500 %,
Temperature -40.0 °C
5313 psi

@Strain 0.500 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G15HSL NC010 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL NC010 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
Tensile Stress 36.63 MPa

@Strain 0.770 %,
Temperature 23.0 °C
5313 psi

@Strain 0.770 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6  (Unverified Data**)
30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..