Polymer Property : Tensile Stress = 531 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 3.66 MPa

@Strain 100 %
531 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® S4465 TPE, PS Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong ..
Tensile Stress 3.66 MPa

@Strain 100 %
531 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® S4665 TPE, PS Overmold
Characteristics: Excellent slip resistanceSoft touchGood weather and heat resistanceEasy processingWide range of hardnessExceptional colorabilityTypical Applications: ConsumerElectronicsHealthcareIn..
Tensile Stress 3.66 MPa

@Strain 32.97 %,
Temperature 90.0 °C
531 psi

@Strain 32.97 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 3.66 MPa

@Strain 0.0500 %,
Temperature 180 °C
531 psi

@Strain 0.0500 %,
Temperature 356 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e..
Tensile Stress 3.66 MPa

@Strain 0.0800 %,
Temperature 220 °C
531 psi

@Strain 0.0800 %,
Temperature 428 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 3.66 MPa

@Strain 0.170 %,
Temperature -40.0 °C
531 psi

@Strain 0.170 %,
Temperature -40.0 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010  (Unverified Data**)
Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s..
Tensile Stress 3.66 MPa

@Strain 14.45 %,
Temperature 60.0 °C
531 psi

@Strain 14.45 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 3.66 MPa

@Strain 59.34 %,
Temperature 150 °C
531 psi

@Strain 59.34 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers