Polymer Property : Tensile Stress = 53.04 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 53.04 MPa

@Strain 1.10 %,
Temperature 80.0 °C
7693 psi

@Strain 1.10 %,
Temperature 176 °F
ISO 11403-1/-2
DuPont Performance Polymers Crastin® LW9330 BK851 PBT  (Unverified Data**)
Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
Tensile Stress 53.04 MPa

@Strain 2.61 %,
Temperature 150 °C
7693 psi

@Strain 2.61 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po..