Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.60 MPa @Strain 300 % |
522 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S EF 70A-3S1975 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Tensile Stress | 3.60 MPa @Strain 300 % |
522 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S FR 50A-3S1831 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Tensile Stress | 3.60 MPa @Strain 300 % |
522 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S HF 70A-3S1984 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tensile Stress | 3.60 MPa @Strain 100 % |
522 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S HF 90A-3S1988 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tensile Stress | 3.60 MPa @Strain 47.25 %, Temperature 100 °C |
522 psi @Strain 47.25 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.60 MPa @Strain 150.02 %, Temperature 120 °C |
522 psi @Strain 150.02 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.60 MPa @Strain 23.55 %, Temperature 90.0 °C |
522 psi @Strain 23.55 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |
|||
Tensile Stress | 3.60 MPa @Strain 98.4 %, Temperature 120 °C |
522 psi @Strain 98.4 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |
|||
Tensile Stress | 3.60 MPa @Strain 300 % |
522 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.60 MPa @Strain 300 % |
522 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.60 MPa @Strain 300 % |
522 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.60 MPa @Strain 300 % |
522 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.60 MPa @Strain 100 % |
522 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P80A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P80A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.60 MPa @Strain 100 % |
522 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P80A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P80A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |