Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 50.61 MPa @Strain 2.20 %, Temperature 23.0 °C |
7341 psi @Strain 2.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by.. |
|||
Tensile Stress | 50.61 MPa @Strain 0.330 %, Temperature 23.0 °C |
7340 psi @Strain 0.330 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 50.61 MPa @Strain 0.890 %, Temperature 90.0 °C |
7340 psi @Strain 0.890 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po.. |