Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 5.90 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 5.90 MPa

@Strain 300 %
856 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S FR 80A-3S1892 Thermoplastic Elastomer (TPE)
OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo..
Tensile Stress 5.90 MPa

@Strain 300 %
856 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3780 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 5.90 MPa

@Strain 0.400 %,
Temperature 90.0 °C
856 psi

@Strain 0.400 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
Tensile Stress 5.90 MPa

@Strain 10.0 %
856 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8068 Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Flame Retardant Polyester Elastomer Developed for Extrusion and Injection Molding Information provided by DuPont Performance Polymers
Tensile Stress 5.90 MPa

@Strain 10.0 %,
Temperature 23.0 °C
856 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET  (Unverified Data**)
Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio..
Tensile Stress 5.90 MPa

@Strain 0.100 %,
Temperature 100 °C
856 psi

@Strain 0.100 %,
Temperature 212 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved