Mechanical Properties Metric English Comments
Tensile Stress 3.30 MPa

@Strain 100 %,
Thickness 2.00 mm
479 psi

@Strain 100 %,
Thickness 0.0787 in
Type 1, 200 mm/min Across Flow; DIN 53504
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE)
OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
Tensile Stress 3.30 MPa

@Strain 300 %
479 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P1770 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 3.30 MPa

@Strain 51.73 %,
Temperature 100 °C
479 psi

@Strain 51.73 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 3.30 MPa

@Strain 0.0600 %,
Temperature 220 °C
479 psi

@Strain 0.0600 %,
Temperature 428 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 3.30 MPa

@Strain 64.05 %,
Temperature 120 °C
479 psi

@Strain 64.05 %,
Temperature 248 °F
ISO 527
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..
Tensile Stress 3.30 MPa

@Strain 100 %,
Temperature 100 °C
479 psi

@Strain 100 %,
Temperature 212 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET  (Unverified Data**)
Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio..
Tensile Stress 3.30 MPa

@Strain 10.0 %
479 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients..