Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 32.0 MPa @Strain 12.0 %, Temperature 160 °C |
4640 psi @Strain 12.0 %, Temperature 320 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 32.0 MPa @Strain 0.900 %, Temperature -20.0 °C |
4640 psi @Strain 0.900 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi.. |
|||
Tensile Stress | 32.0 MPa @Strain 8.50 %, Temperature 90.0 °C |
4640 psi @Strain 8.50 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem.. |
|||
Tensile Stress | 32.0 MPa @Strain 2.00 %, Temperature 23.0 °C |
4640 psi @Strain 2.00 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide .. |
|||
Tensile Stress | 32.0 MPa @Strain 4.70 %, Temperature 90.0 °C |
4640 psi @Strain 4.70 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |
|||
Tensile Stress | 32.0 MPa @Strain 300 % |
4640 psi @Strain 300 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 32.0 MPa @Strain 0.600 %, Time 3.60e+7 sec |
4640 psi @Strain 0.600 %, Time 10000 hour |
ISO 899-1 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Tensile Stress | >= 32.0 MPa @Strain 300 % |
>= 4640 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 372D Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tensile Stress | >= 32.0 MPa @Strain 300 % |
>= 4640 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 772D PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tensile Stress | >= 32.0 MPa @Strain 300 % |
>= 4640 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 598A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tensile Stress | 32.0 MPa @Strain 5.60 %, Temperature 40.0 °C |
4640 psi @Strain 5.60 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |