Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 31.6 MPa @Strain 1.33 %, Temperature 23.0 °C |
4580 psi @Strain 1.33 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal.. |
|||
Tensile Stress | 31.6 MPa @Strain 1.20 %, Temperature 23.0 °C |
4580 psi @Strain 1.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi.. |
|||
Tensile Stress | 31.6 MPa @Strain 2.02 %, Temperature 150 °C |
4580 psi @Strain 2.02 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66
(Unverified Data**) 20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf.. |