Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S EH 60A-3S7003 Thermoplastic Elastomer (TPE) OnFlex™-S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S FR 40A-3S1841 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Tensile Stress | 3.10 MPa @Strain 100 % |
450 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® C4970M TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 3.10 MPa @Strain 100 %, Temperature 23.0 °C |
450 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ HC MT317 Thermoplastic Elastomer (TPE) Versaflex™ HC MT317 is an extrudable, sterilizable TPE developed for medical tubing applications in healthcare. - Autoclavable sterilizable - Flexible - Kink Resistant New product. Commercial speci.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 %, Temperature 23.0 °C |
450 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7970-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9065 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 %, Temperature 23.0 °C |
450 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 %, Temperature 23.0 °C |
450 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 %, Temperature 23.0 °C |
450 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tensile Stress | 3.10 MPa @Strain 100 % |
450 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Telcar® TELC 302 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Stress | 3.10 MPa @Strain 100 % |
450 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Telcar® TL-4001A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Stress | 3.10 MPa @Strain 0.100 %, Temperature 60.0 °C |
450 psi @Strain 0.100 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66
(Unverified Data**) Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP.. |
|||
Tensile Stress | 3.10 MPa @Strain 0.150 %, Temperature -20.0 °C |
450 psi @Strain 0.150 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ P50A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P50A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.10 MPa @Strain 300 % |
450 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ P50A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P50A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.10 MPa @Strain 100 % |
450 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P75A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P75A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.10 MPa @Strain 100 % |
450 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P75A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P75A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |