Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 29.0 MPa @Strain 2.54 %, Temperature 23.0 °C |
4210 psi @Strain 2.54 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 29.0 MPa @Strain 2.50 %, Temperature 23.0 °C |
4210 psi @Strain 2.50 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 29.0 MPa @Strain 0.140 %, Temperature -40.0 °C |
4210 psi @Strain 0.140 %, Temperature -40.0 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Tensile Stress | 29.03 MPa @Strain 0.800 %, Temperature 150 °C |
4210 psi @Strain 0.800 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per.. |
|||
Tensile Stress | 29.0 MPa @Strain 0.700 %, Temperature 150 °C |
4210 psi @Strain 0.700 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon
(Unverified Data**) Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve.. |
|||
Tensile Stress | 29.0 MPa @Strain 3.70 %, Temperature 90.0 °C |
4210 psi @Strain 3.70 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Stress | 29.0 MPa @Strain 50.0 % |
4210 psi @Strain 50.0 % |
DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010 Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced.. |
|||
Tensile Stress | 29.0 MPa @Strain 3.00 %, Time 360000 sec |
4210 psi @Strain 3.00 %, Time 100 hour |
ISO 899-1 |
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |
|||
Tensile Stress | 29.0 MPa @Strain 50.0 %, Temperature 120 °C |
4210 psi @Strain 50.0 %, Temperature 248 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |