Mechanical Properties Metric English Comments
Tensile Stress 42.6 MPa

@Strain 13.4 %,
Temperature 40.0 °C
6180 psi

@Strain 13.4 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AF Acetal (POM)  (Unverified Data**)
20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi..
Tensile Stress 42.6 MPa

@Strain 1.20 %,
Temperature 0.000 °C
6180 psi

@Strain 1.20 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem..
Tensile Stress 42.6 MPa

@Strain 2.83 %,
Temperature 180 °C
6180 psi

@Strain 2.83 %,
Temperature 356 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G35HSLR BK031 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR BK031 is a 35% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i..